Product : High Tensile Reclaimed Rubber

Grade : KRHT

Properties

Units

Limits

Test Result

Chemical Properties

Acetone Extract

%

14 + 3

14.80

Ash Content

%

7 + 2

7.20

Carbon Black

%

28 + 3

27.80

RHC By Difference

%

Min 47

49.90

Physical Properties

Specific Gravity

gm / cc

Max. 1.15

1.13

Tensile Strength

kg / cm²

Min 65

70

Elongation At Break

%

Min 250

321

Hardness

Shore 'A'

59 + 3

60

Mooney Viscosity

ML( 1+4) @ 100oC (At the time of Mfg.)

35-60

58


Trade Information
  • Payment Terms
  • Telegraphic Transfer (T/T)
  • Delivery Time
  • as per requirement Days
  • Main Export Market(s)
  • Africa, Middle East, Western Europe, Eastern Europe, South America, North America, Central America, Australia, Asia
  • Main Domestic Market
  • All India

KAPOOR OIL MILLS
X


KAPOOR OIL MILLS All Rights Reserved.